May 01, 2018 · Qiao, X C; Si, P; Yu, J G.-15. This research has applied kaolin and active carbon (AC) to the investigation of the recovery of aluminum from coal spoil (CS). The kaolin, AC-containing kaolin mixture, and CS have been calcined at 500, 600, 700, 800, and 900 degrees C for 15, 30, 60, and 120 min.