Jan 04, 2021 · Guo et al. dissolved FeSO 4 ·7H 2 O in water, stirred it vigorously at room temperature, and added Na 2 S 2 O 3 and then NaOH drop by drop. Finally, the solution was heated for 12 h at 413 K. The size of MFNs was within the range of 80–120 nm, and the magnetization saturation value was 57.59 emu/g. Solvothermal method